Usually caused by selvage being stretched in finishing or by uneven wetting out in sanforization process.
What is “Puckered Selvage”
Usually caused by selvage being stretched in finishing or by uneven wetting out in sanforization process.
Note: This content is for informational purposes only. Please read our full disclaimer for more details.
Some more terms:
Plaid in Textiles: Discover Its Evolution and Future Trends
Plaid is a textile pattern characterized by a crisscrossing of horizontal and vertical lines of different widths and colors, forming squares or rectangles of different sizes. It is a traditional...
Read about Plaid
The Art of Flocking: Applying Soft, Raised Surfaces for Visual Appeal
Flocking is a decorative textile finishing process that involves applying small fibers, called flock, to a surface to create a soft, velvet-like texture. Flocking can be applied to a wide range of...
Read about Flocking
Crocking in Textiles: Understanding Color Transfer and How to Prevent It
In textiles, crocking refers to the tendency of dyes or pigments to rub off or transfer onto other surfaces, particularly when the fabric is rubbed or abraded. Crocking can occur in both natural and...
Read about Crocking
Folded Yarns: Twisting Multiple Strands for Enhanced Strength in Fashion and Industry
Folded yarn, also known as cabled yarn, is a type of yarn that is created by twisting two or more plies of yarn together in the opposite direction from which they were spun. This process, called...
Read about Folded yarn